Effect of C@SiC Composite Powder Addition on Properties of Al2O3-SiC-C Castables for Iron Trough
文献摘要:
Al2O3-SiC-C castables were prepared using C@SiC composite powder modified by molten salts to replace ball pitch gradually.The effects of the C@SiC composite powder addition(0,1%,1.5%,and 2%,by mass)on the water requirement,the flow value,the physical properties,the thermal shock resistance,the oxidation resistance,and the corrosion resistance of castables were studied.The results show that with the C@SiC addition increasing,the amount of water added to the castable increases,but the apparent porosity of the samples after heat treatment first increases and then decreases,and the cold modulus of rupture increases significantly.After completely replacing the ball pitch,the cold modulus of rupture of the sample increases by 51.2%,and the residual strength ratio increases by 28.7%.In addition,the sample with 2%C@SiC has the best oxidation resistance,and the sample with 1.5%C@SiC composite powder has the smallest corrosion depth.
文献关键词:
作者姓名:
LIU Zhenglong;DENG Chengji;YU Chao;DING Jun;ZHU Hongxi
作者机构:
The State Key Laboratory of Refractories and Metallurgy,Wuhan University of Science and Technology,Wuhan 430081,China
引用格式:
[1]LIU Zhenglong;DENG Chengji;YU Chao;DING Jun;ZHU Hongxi-.Effect of C@SiC Composite Powder Addition on Properties of Al2O3-SiC-C Castables for Iron Trough)[J].中国耐火材料(英文版),2022(04):39-44
A类:
Castables,castables,castable
B类:
Effect,SiC,Composite,Powder,Addition,Properties,Al2O3,Iron,Trough,were,prepared,using,composite,powder,modified,by,molten,salts,replace,ball,pitch,gradually,effects,addition,mass,water,requirement,flow,value,physical,properties,thermal,shock,resistance,oxidation,corrosion,studied,results,show,that,increasing,amount,added,increases,but,apparent,porosity,samples,after,heat,treatment,first,then,decreases,cold,modulus,rupture,significantly,After,completely,replacing,residual,strength,ratio,In,has,best,smallest,depth
AB值:
0.519158
相似文献
Selective Laser Melting of Al-7Si-0.5 Mg-0.5Cu:Effect of Heat Treatment on Microstructure Evolution,Mechanical Properties and Wear Resistance
Pei Wang;Sijie Yu;Jaskarn Shergill;Anil Chaubey;Jurgen Eckert;Konda Gokuldoss Prashanth;Sergio Scudino-Additive Manufacturing Institute,College of Mechatronics and Control Engineering,Shenzhen University,Shenzhen 518060,China;Institute for Complex Materials,IFW Dresden,Helmholtzstra?e 20,01069 Dresden,Germany;Institute of Minerals and Materials Technology(IMMT),Bhubaneshwar 751013,Orissa,India;Erich Schmid Institute of Materials Science,Austrian Academy of Sciences,Jahnstra?e 12,8700 Leoben,Austria;Department of Materials Science,Chair of Materials Physics,Montanuniversit?t Leoben,Jahnstra?e 12,8700 Leoben,Austria;Adjunct With National University of Science and Technology ?MISiS?,Leninsky Prosp.,4,119049 Moscow,Russia;Department of Mechanical and Industrial Engineering,Tallinn University of Technology,Ehitajete tee 5,19086 Tallinn,Estonia;CBCMT,School of Mechanical Engineering,Vellore Institute of Technology,Vellore,Tamil Nadu 632 014,India
机标中图分类号,由域田数据科技根据网络公开资料自动分析生成,仅供学习研究参考。