Microstructure of Bi-containing zirconium alloys
文献摘要:
The effect of Bi addition(0.05 wt%-0.50 wt%)on the microstructure of zirconium alloys,including T5(Zr-0.7Sn-1.0Nb-0.3Fe-0.1Cr),S5(Zr-0.8Sn-0.35Nb-0.4Fe-0.1Cr),Zr-4(Zr-1.5Sn-0.2Fe-0.1Cr)and Zr-1Nb,was investigated by transmission electron microscopy(TEM),energy-dispersive spectroscopy(EDS)and selected area electron diffraction(SAED).Results show that with the increase in Bi content,h-Zr(Fe,Cr,Nb)2,o-Zr(Fe,Sn,Bi)2 and Zr-Fe-Cr-Nb-Sn-Bi second-phase particles(SPPs)precipitate successively in the T5+xBi and S5+xBi alloys;in the Zr-4+xBi alloys,h-Zr(Fe,Cr)2,o-Zr(Fe,Sn,Bi)2,Zr-Fe-Cr-Sn-Bi and Zr-Fe-Cr-Bi SPPs are detected successively.While as for Zr-1Nb+xBi alloys,Bi-free SPPs appear.The addition of Bi promotes the precipitation of SPPs with Sn in the alloys.The con-centration of Bi dissolved in α-Zr matrix increases with the decrease in Sn content in the alloys.Adding reasonable Bi has little influence on the solid solution content of Nb in α-Zr matrix.
文献关键词:
作者姓名:
Han-Pei Zhao;Mei-Yi Yao;Jiao Huang;Jin-Long Zhang;Jian-Chao Peng;Bang-Xin Zhou
作者机构:
Laboratory for Microstructure,Shanghai University,Shanghai 200444,China;Institute of Materials,Shanghai University,Shanghai 200072,China
引用格式:
[1]Han-Pei Zhao;Mei-Yi Yao;Jiao Huang;Jin-Long Zhang;Jian-Chao Peng;Bang-Xin Zhou-.Microstructure of Bi-containing zirconium alloys)[J].稀有金属(英文版),2022(10):3566-3573
A类:
T5+xBi,S5+xBi,4+xBi,1Nb+xBi
B类:
Microstructure,containing,zirconium,alloys,effect,addition,wt,microstructure,including,Zr,7Sn,0Nb,3Fe,1Cr,8Sn,35Nb,4Fe,5Sn,2Fe,was,investigated,by,transmission,electron,microscopy,TEM,energy,dispersive,spectroscopy,EDS,selected,area,diffraction,SAED,Results,show,that,content,second,phase,particles,SPPs,precipitate,successively,detected,While,free,appear,promotes,precipitation,centration,dissolved,matrix,increases,decrease,Adding,reasonable,little,influence,solid,solution
AB值:
0.422662
相似文献
Influence of Zr and Mn additions on microstructure and properties of Mg–2.5wt%Cu–Xwt%Zn (X = 2.5, 5 and 6.5) alloys
A.V.Koltygin;V.E.Bazhenov;I.V.Plisetskaya;V.A.Bautin;A.I.Bazlov;N.Y.Tabachkova;O.O.Voropaeva;A.A.Komissarov;V.D.Belov-Foundry Department,National University of Science and Technology(MISiS),Moscow 119049,Russia;Department of Metallurgy Steel,New Production Technologies and Protection of Metals,National University of Science and Technology(MISiS),Moscow119049,Russia;Laboratory of Advanced Green Materials,National University of Science and Technology(MISiS),Moscow 119049,Russia;Department of Materials Science of Semiconductors and Dielectrics,National University of Science and Technology(MISiS),Moscow 119049,Russia;Fianit Laboratory(Laser Materials and Technology Research Center at GPI),Prokhorov General Physics Institute RAS,Moscow 119991,Russia;Laboratory of Hybrid Nanostructured Materials,National University of Science and Technology(MISiS),Moscow 119049,Russia;Laboratory of Medical Bioresorption and Bioresistance,Moscow State University of Medicine and Dentistry,Moscow 127473,Russia
Microstructure evolution and deformation mechanism of α+β dual-phase Ti-xNb-yTa-2Zr alloys with high performance
Ting Zhang;Daixiu Wei;Eryi Lu;Wen Wang;Kuaishe Wang;Xiaoqing Li;Lai-Chang Zhang;Hidemi Kato;Weijie Lu;Liqiang Wang-State Key Laboratory of Metal Matrix Composites,School of Material Science and Engineering,Shanghai Jiao Tong University,Shanghai,200240,China;School of Metallurgical Engineering,Xi'an University of Architecture and Technology,Xi'an,710055,China;Institute for Materials Research,Tohoku University,2-1-1 Katahira,Sendai,Miyagi,980-8577,Japan;Department of Stomatology,Renji Hospital,School of Medicine,Shanghai Jiao Tong University,Shanghai,200127,China;Department of Materials Science and Engineering,KTH-Royal Institute of Technology,10044,Stockholm,Sweden;School of Engineering,Edith Cowan University,270 Joondalup Drive,Joondalup,Perth,WA 6027,Australia
机标中图分类号,由域田数据科技根据网络公开资料自动分析生成,仅供学习研究参考。